COATING WEIGHTS FOR ONE-MIL
THICK DEPOSITS
This table gives the gage pressure of saturated
steam in pounds per square inch corresponding to the stated
temperature.
Zero gage pressure is equal to 14.70 pounds per square inch absolute.
|
METAL |
oz./sq. ft. |
mg/sq. in. |
mg/sq. cm. |
| Aluminum |
0.225 |
44.7 |
6.9 |
| Antimony |
0.557 |
111 |
17.0 |
| Arsenic |
0.475 |
94.3 |
14.5 |
| Bismuth |
0.816 |
162 |
24.9 |
| Cadmium |
0.72 |
143 |
22.0 |
| Chromium |
0.591 |
117 |
18.0 |
| Cobalt |
0.74 |
147 |
22.6 |
| Copper |
0.74 |
147 |
22.6 |
| Gallium |
0.491 |
97.5 |
15.0 |
| Germanium |
0.445 |
88.3 |
13.6 |
| Gold |
1.61 |
320 |
49.2 |
| Indium |
0.608 |
121 |
18.6 |
| Iridium |
1.869 |
368 |
57.0 |
| Iron |
0.66 |
130 |
20.1 |
| Lead |
0.94 |
185 |
28.7 |
| Manganese |
0.598 |
118 |
18.2 |
| Nickel |
0.742 |
146 |
22.6 |
| Palladium |
0.998 |
196 |
30.4 |
| Platinum |
1.78 |
350 |
54.3 |
| Rhodium |
1.04 |
205 |
31.8 |
| Rhenium |
1.71 |
336 |
52.2 |
| Selenium |
0.400 |
78.7 |
12.2 |
| Silver |
0.875 |
172 |
26.7 |
| Tellurium |
0.520 |
102 |
15.9 |
| Thallium |
0.986 |
194 |
30.1 |
| Tin |
0.61 |
120 |
18.6 |
| Zinc |
0.59 |
116 |
18.0 |
|